SamplePP-WT-016
Plastic Type Polypropylene (PP)
Molecular Formula(C3H6)n
ColorWhite
Common useUnknown
Degradation detailsExposure to environmental conditions such as dust, dirt, temperature
variations (without exposure to sun radiation) and to mechanical stress.
Time of degradation4 years
Sample descriptionRigid, yellowish sample covered with dirt, dust and scratches. It shows visible signs of degradation.
Microscopic image(s)
Macroscopic image(s)
Spectral Data typeRaman
Raman spectrum
acquisition parameters
Laser wavelength: 785 nm
Laser Power: 300 mW (100% of the laser power)
Exposure time: 1 s
Objective magnification: 20X (NA 0.35)
Spectrum range: 765-1600 cm-1