SamplePP-WT-001
Plastic Type Polypropylene (PP)
Molecular Formula(C3H6)n
ColorWhite
Common useSurgical mesh
Degradation detailsThe sample was introduced in liquid nitrogen for 15 minutes and then crushed with a hammer
Time of degradation15 minutes
Sample descriptionThe sample is flexible with visible signs of degradation. It was flattened after the degradation process.
Microscopic image(s)
Macroscopic image(s)
Spectral Data typeRaman
Raman spectrum
acquisition parameters
Laser wavelength: 785 nm
Laser Power: 300 mW (100% of the laser power)
Exposure time: 1 s
Objective magnification: 20X (NA 0.35)
Spectrum range: 765-1600 cm-1