Sample | PP-BL-001 |
Plastic Type | Polypropylene (PP) |
Molecular Formula | (C3H6)n |
Color | Blue |
Common use | Surgical mesh |
Degradation details | The sample was introduced in liquid nitrogen for 15 minutes and then crushed with a hammer |
Time of degradation | 15 minutes |
Sample description | The sample is flexible with visible signs of degradation. It was flattened after the degradation process. |
Microscopic image(s) | |
Macroscopic image(s) | |
Spectral Data type | Raman |
Raman spectrum acquisition parameters | Laser wavelength: 785 nm Laser Power: 300 mW (100% of the laser power) Exposure time: 1 s Objective magnification: 20X (NA 0.35) Spectrum range: 765-1600 cm-1 |