Sample | PP-RD-003 |
Plastic Type | Polypropylene (PP) |
Molecular Formula | (C3H6)n |
Color | Red |
Common use | Lid for mustard jar |
Degradation details | Exposure to indoor conditions for 2 years (no exposure to aggresive environmental conditions) . After indoor degradation, the sample was degraded in environmental conditions (for 3 months) such as wind, rain, snow, temperature variations and sun radiation |
Time of degradation | 2 years of indoor degradation + 3 months of environemntal degradation |
Sample description | After the environmetal degradation it was covered with dirt and few scratches. |
Microscopic image(s) | |
Macroscopic image(s) | |
Spectral Data type | Raman |
Raman spectrum acquisition parameters | Laser wavelength: 785 nm Laser Power: 300 mW (100% of the laser power) Exposure time: 1 s Objective magnification: 20X (NA 0.35) Spectrum range: 765-1600 cm-1 |