Sample | PP-TP-005 |
Plastic Type | Polypropylene (PP) |
Molecular Formula | (C3H6)n |
Color | Transparent |
Common use | Toothpicks container |
Degradation details | Exposure to indoor conditions for 2 years: exposure to temperatures around 45 oC, but no exposure to aggresive environmental factors. |
Time of degradation | 2 years |
Sample description | The sample is yellowish. |
Microscopic image(s) | |
Macroscopic image(s) | |
Spectral Data type | Raman |
Raman spectrum acquisition parameters | Laser wavelength: 785 nm Laser Power: 300 mW (100% of the laser power) Exposure time: 1 s Objective magnification: 20X (NA 0.35) Spectrum range: 765-1600 cm-1 |