SamplePP-WT-003
Plastic Type Polypropylene (PP)
Molecular Formula(C3H6)n
ColorWhite
Common useDisposable plastic cup
Degradation detailsExposure to environmental conditions (it was in contact with soil for a long time) + the sample was introduced in liquid nitrogen for 15 minutes and then crushed (flattened) with a hammer
Time of degradation10 years of environmental degradation + 15 minutes of accelerated degradation conditions in the laboratory
Sample descriptionThe sample shows visible signs of degradation (it is covered with dirt). After the liquid nitrogen treatment, the sample was very fragile to mechanical stress and broke very easily into small piecies
Microscopic image(s)
Macroscopic image(s)
Spectral Data type Raman
Raman spectrum acquisition parametersLaser wavelength: 785 nm
Laser Power: 300 mW (100% of the laser power)
Exposure time: 1 s
Objective magnification: 20X (NA 0.35)
Spectrum range: 765-1600 cm-1