SamplePP-WT-002
Plastic Type Polypropylene (PP)
Molecular Formula(C3H6)n
ColorWhite
Common useDisposable plastic cup
Degradation detailsExposure to environmental conditions (it was in contact with soil for a long time)
Time of degradation10 years
Sample descriptionThe sample shows visible signs of degradation; it is covered with dirt being very fragile due to degradation.
Microscopic image(s)
Macroscopic image(s)
Spectral Data typeRaman
Raman spectrum
acquisition parameters
Laser wavelength: 785 nm
Laser Power: 300 mW (100% of the laser power)
Exposure time: 1 s
Objective magnification: 20X (NA 0.35)
Spectrum range: 765-1600 cm-1