SamplePP-PK-001
Plastic Type Polypropylene (PP)
Molecular Formula(C3H6)n
ColorPink
Common useCap for Vanish bottle
Degradation detailsExposure to environmental conditions (for 3 months) such as wind, rain, snow, temperature variations and sun radiation.
Time of degradation3 months
Sample descriptionAfter degradation, the sample was covered with dirt and scratches showing few visible signs of degradation.
Microscopic image(s)
Macroscopic image(s)
Spectral Data typeRaman
Raman spectrum acquisition parametersLaser wavelength: 785 nm
Laser Power: 300 mW (100% of the laser power)
Exposure time: 1 s
Objective magnification: 20X (NA 0.35)
Spectrum range: 765-1600 cm-1